WATERPROOFING MEMBRANE

T-1000

  • - Test: tensile strength (longitudinal), method: EN-12311, unit: N/5CM, typical values: 640.
  • - Test: tensile strength (transverse), method: EN-12311, unit: N/5CM, typical values: 560
  • - Test: tear resistance (longitudinal), method: ASTM D-5147, D 4073, unit: N, typical values: 400.
  • - Test: tear resistance (transverse), method: ASTM D-5147, D 4073, unit: N, typical values: 400.
  • - Test: Softening point, method: ASTM D-36, unit:℃, typical values: 150.